WHEN copper alloys containing more than 2 per cent aluminium were heated for many hours at a red heat (800°–900° C), no oxide scales were formed. In cases where several per cent of this element was added, the alloys even retained their characteristic golden yellow lustre, which is a very remarkable fact. Elements such as tin, zinc, nickel, manganese, magnesium, iron, etc., when added to copper do not produce this effect.
Similar content being viewed by others
Article PDF
References
G. P. Thomson, Proc. Roy. Soc., A, 128, 649; 1930. C. A. Murison, Phil. Mag., 17, 96; 1934.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
IITAKA, I., MIYAKE, S. Oxide Film of Alloys containing Small Percentages of Aluminium. Nature 136, 437 (1935). https://doi.org/10.1038/136437a0
Issue Date:
DOI: https://doi.org/10.1038/136437a0
This article is cited by
-
The high-temperature oxidation of some oxidation-resistant copper-based alloys
Oxidation of Metals (1971)
-
Selective Oxidation of Aluminium Alloys
Nature (1939)
-
Adsorption of Constituents of a Solid Phase on the Surface
Nature (1938)
Comments
By submitting a comment you agree to abide by our Terms and Community Guidelines. If you find something abusive or that does not comply with our terms or guidelines please flag it as inappropriate.