Table 2: The raw biosensor data, the calculated adsorbed polyphenol mass and the number of formed polyphenol layers on the PP:PPR coating for three different concentrations.

From: Green tea polyphenol tailors cell adhesivity of RGD displaying surfaces: multicomponent models monitored optically

 Conc. (μg/ml)Δλ (pm)ΔM (ng/cm2)Number of layers
EGCg5480.94 ± 4.81129.64 ± 1.293.43 ± 0.03
50689 ± 87.49185.73 ± 23.584.91 ± 0.62
500797.39 ± 140.50214.94 ± 37.865.68 ± 1.00
Ox. EGCg5354.3 ± 8.2495.5 ± 2.212.52 ± 0.05
50969.04 ± 33.55261.21 ± 9.046.91 ± 0.23
5001535.54 ± 41.46413.92 ± 11.1710.95 ± 0.29