Figure 4

From: Green tea polyphenol tailors cell adhesivity of RGD displaying surfaces: multicomponent models monitored optically

Figure 4

The recorded kinetic curves when the PP coating was exposed to EGCg and oxidized EGCg solutions with various concentrations (A,E). The concentration dependence of the finally adsorbed amounts are shown separately (B,F). The biosensor signals were recorded after cell addition onto the polyphenol exposed coatings. For comparison, the cell spreading curves recorded on the PP:PPR cell adhesive coating are also shown (C,G). The applied concentrations of EGCg and oxidized EGCg were 0, 0.05, 0.5, 5, 20, 40, 50, 500 μg/ml and indicated in the graphs. The concentration dependence of the cell adhesion signals after 2 hours of cell addition (D,H).