Figure 2 | Scientific Reports

Figure 2

From: Replication of a Printed Volatile Mold: a novel microfabrication method for advanced microfluidic systems

Figure 2

Demonstration of (a) hexanediol pattern printed on glass (temperature substrate 5 \({}^{\circ }\)C) and (b) the final chip filled with red dye. The channel width is 50 \(\mu \)m. This chip was used directly after ink removal, ie without plasma bonding. (c) Non-flat cellulose acetate filter paper (temperature substrate 5 \({}^{\circ }\)C). (d) Uncross-linked liquid PDMS (temperature substrate −24 \({}^{\circ }\)C). Scale bars 2 mm.