High-temperature test rigs used in this study. (a) Closed loop test system with a vacuum chamber; the load cell (L) and front glass window (GW) are highlighted. (b) Extensometer system placed in front of the GW. (c) Open vacuum chamber with a specimen (down arrow) and thermocouples (T) highlighted. (d) A specimen and graphite loading grips. The widths of the two gaps, Δ1 and Δ2, are recorded during creep testing.