Figure 7 | Scientific Reports

Figure 7

From: Ultrahigh-temperature tensile creep of TiC-reinforced Mo-Si-B-based alloy

Figure 7

SEM image montages taken after creep deformation at 1500 °C and 137 MPa. (a) Overview montage of SEM micrographs after short creep exposure (2.9%, 4.3 h). (b) Higher magnification SEM image from the region indicated by the dashed rectangle in Fig. 7(a) showing that small pores form in the early stages of creep. (c) Overview montage of SEM micrographs after rupture (72%, 44 h).