Table 1 Pore size and the thickness of the branch listed as function of mixing ratio.

From: In-situ Observation of Hierarchical Self-Assembly Driven by Bicontinuous Gelation in Mixed Nanodisc Dispersions

Mixing ratio ( r ) 10 5 4 3 2.5
Area (μm2)    SEM                          Confocal 25 ± 7 29 ± 11 3 ± 0.5 3 ± 0.7 1.3 ± 0.4 1.5 ± 0.5 47 ± 17 51 ± 20 97 ± 20, 17 ± 4            —
Thickness of branches (nm) 123 ± 3.5 70 ± 17 35 ± 8 2203 ± 300 300 ± 60, 101 ± 10