Fig. 3 | npj Materials Degradation

Fig. 3

From: Localized corrosion of low-carbon steel at the nanoscale

Fig. 3

Examination of 1018 steel region that experienced localized corrosion. Scale bar indicates 200 nm. Aligned and averaged in-situ a BF-STEM and b HAADF-STEM images showing accelerated corrosion at the phase boundary between ferrite and cementite. Four images over a 6 min period were averaged