Surface analysis of the Li anodes after cycling in Li-O2 cells. a, b SEM images of the Li anode after the 60 cycles with 50 mM TESI. Scale bars are 4 μm (a) and 2 μm (b). c SEM image of the Li anode after 30 cycles with 50 mM LiI. Scale bar is 4 μm. d FTIR spectra on the surface of the Li anode after 1 cycle and 60 cycles with 50 mM TESI additive