Figure 2

(a) Evolution of open-circuit voltage (VOC), fill factor (FF), short-circuit current density (JSC) and power conversion efficiency (PCE) of an optimized PCE11:PCBM solar cell measured under continuous 1 sun equivalent illumination (in N2 atmosphere) for 450 h. (b) Evolution of JSC of optimized PCE11:PCBM solar cells measured at different temperatures.