Extended Data Figure 6 : Micrographs of etched Al6061, processed as received.

From: 3D printing of high-strength aluminium alloys

Extended Data Figure 6

Large cracks are observed in the absence of Zr (left). With the addition of Zr nanoparticles, no cracking is observed, but there is some residual porosity (right). Rows indicate increasing magnification.