Extended Data Figure 3 : Lap-shear test of PDMA S0.1 gels glued by various particle solutions.

From: Nanoparticle solutions as adhesives for gels and biological tissues

Extended Data Figure 3

In order of increasing deformation at the breaking point are shown the adhesive failure by interfacial peeling in CNT-Thy (grey), CNC1 (green), SM-30 (yellow) and HS-40 (purple). Fracture outside the junction occurred for TM-50 (blue) and AL-30 (red). Lap-joint dimensions were l = 5 mm, w = 5 mm and h = 2 mm. 6 μl of solution was spread to make the junction.