Advanced analytical electron microscopy for lithium-ion batteries

Danna Qian, Cheng Ma, Karren L More, Ying Shirley Meng and Miaofang Chi

BACK TO ARTICLE

Figure 6.

Unfortunately we are unable to provide accessible alternative text for this. If you require assistance to access this image, please contact help@nature.com or the author

(a) Schematic of the liquid-cell configuration.63 (b, c) In situ observation of the inhomogeneous lithiation, the lithium metal dendritic growth, and the solid–electrolyte interface formation.22 (d) An example of the all-solid-state microbattery with the configuration of Au (current collector)/SnO2 (anode)/Li3.4V0.6Si0.4O4 (electrolyte)/LiNi0.5Mn1.5O4 (cathode)/Pt (current collector).67 (e, f) The EELS mapping of Ni, V, Li and Li intensity of the microbattery in (d).67 All figures have been reproduced with permission.